2K Gloss
#1
Posted 12 October 2017 - 07:09 PM
I am unsure if as temps are below 25 deg if fast thinner is best
Thanks
#2
Posted 12 October 2017 - 07:12 PM
Can anyone confirm what speed of thinners is best for 2k gloss
I am unsure if as temps are below 25 deg if fast thinner is best
Thanks
In my workshop i have used fast activator with standard thinners on 2k. Worked well and that was last weekend.
#3
Posted 12 October 2017 - 07:29 PM
#4
Posted 12 October 2017 - 07:33 PM
Ben_O on here recommends you warm the panels up as much as you can. i had a couple of heaters on in the workshop for an hour and 30 mins or so which helped as well.
#5
Posted 12 October 2017 - 07:35 PM
The dust free times can be speeded up by the addition of a capful of Rocket additive ,
available from paint suppliers! quite useful for cold conditions when air drying 2K.
#6
Posted 12 October 2017 - 08:07 PM
I have built a pretty good booth with filtered inlet and outlet so hopefully dust is not a major problem. I was just concerned with the slow thinners on vertical panels but will see how I go. think I will put heater in garage for an hour or so before I start can only help although it's supposed to be warm this weekend
#7
Posted 12 October 2017 - 08:13 PM
Thanks,
I have built a pretty good booth with filtered inlet and outlet so hopefully dust is not a major problem. I was just concerned with the slow thinners on vertical panels but will see how I go. think I will put heater in garage for an hour or so before I start can only help although it's supposed to be warm this weekend
My bonnet
and boot lid
These were last Saturday and both came up really well. Doors as well